Home / Current Issue / Paper 1725546
Investigating the Effect of Metakaolin on the Flow, Compressive Strength and Water Absorption of High Performance Concrete
Subject area: Science,Engineering and Technology · Area of research: High Performance Concrete; Metakaolin
Abstract
High performance concrete (HPC) requires high binder contents, thereby increasing cost and CO₂ emissions. Metakaolin (MK) from locally available kaolin is a promising partial cement replacement, but its interaction with superplasticiser, water-cement ratio and aggregate-cement proportions in Portland-limestone cement HPC has not been fully investigated. This study examined the combined effect of five mix variables on the fresh, mechanical and durability properties of MK-HPC and identified mixes balancing flow, strength and impermeability. A five-factor, five-level central composite design (60 runs) varied MK (5-15% cement replacement), PCE superplasticiser (1.00-1.20%), water-cement ratio (0.31-0.35), coarse to fine aggregate ratio (0.60-1.00) and cement to fine aggregate ratio (1.10-1.50), using cement and metakaolin. Slump flow, 28-day compressive strength and water absorption of HPC were determined. The results revealed that slump flow ranged from 665 to 730 mm, placing every mix within EFNARC class SF2. Compressive strength ranged from 20.9 to 55.3 MPa, while water absorption value ranges from 0.09-1.17%. Concrete specimen that had 28 days compressive strength above 55 N/mm² was achieved by mixes containing (MK= 10-12.5%, SP = 1.1-1.15%, W/C = 0.32-0.33, CA = 0.9-1.0, CE = 1.3-1.4).
Keywords
central composite design, compressive strength, high-performance concrete, metakaolin, polycarboxylate superplasticizer
References
[1] Abiodun Y, Orisaleye J, Adeosun S (2023). Effect of calcination temperatures of kaolin on compressive and flexural strengths of metakaolin-concrete. Nigerian Journal of Technological Development, 20(1), 33–43.
[2] Agboola S, Abbas K, Musa A, Shabi M, Abdulwaheed A, Zakari A (2024). Performance of concrete using metakaolin as cement partial replacement material. Arid Zone Journal of Engineering, Technology and Environment, 20(4), 749–759.
[3] Aïtcin PC, Flatt RJ (2015). Science and technology of concrete admixtures. Woodhead publishing.
[4] Akinpelu MA, Salman A, Jimoh Y, Yahaya IT, Salami HM (2024). Impact of treatment temperature of metakaolin on strength and sulfate resistance of concrete. Res Eng Struct Mat, 10(3), 1261–1279.
[5] Arslan F, Benli A, Karatas M (2020). Effect of high temperature on the performance of self-compacting mortars produced with calcined kaolin and metakaolin. Construction and Building Materials, 256, 119497.
[6] ASTM-C33 (2018). Standard Specification for Concrete Aggregates. ASTM International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA, 19428-2959 USA.
[7] ASTM-C494 (2017). Standard and Specification for Chemical Admixtures for Concrete. ASTM International, West Conshohocken, PA.
[8] BS-812-110 (1990). Methods for determination of aggregate crushing value (ACV). British Standard Institution, London.
[9] BS-812:2 (1995). Method of determination of particle density, water absorption, and bulk density in aggregate.
[10] BS-1881-116 (1983). Method for determination of compressive strength of concrete cubes, British Standard Institution, London.
[11] BS-EN-196-3 (2016). Methods of testing cement. Determination of setting times and soundness.
[12] BS-EN-206 (2013). Concrete [Internet]. Specification, performance, production and conformity; 2013. Available from: https://knowledge.bsigroup.com/products/concrete-specification-performance-production-and-conformity-2?version=standard
[13] BS-EN-12350-8 (2019). Testing fresh concrete - Self-compacting concrete [Internet]. Slump-flow test; 2019. Available from: https://knowledge.bsigroup.com/products/testing-fresh-concrete-self-compacting-concrete-slump-flow-test?version=tracked
[14] BS-EN-12390-3 (2009). Testing hardened concrete.
[15] BS-EN:196-6 (2018). Methods of testing cement - Determination of fineness [Internet]. 2018. Available from: https://knowledge.bsigroup.com/products/methods-of-testing-cement-determination-of-fineness
[16] BS-EN:12620 (2013). Aggregates for concrete [Internet]. 2013. Available from: https://knowledge.bsigroup.com/products/aggregates-for-concrete-1
[17] Chahar AS, Pal P (2023). A review on various aspects of high performance concrete. Innovative Infrastructure Solutions, 8(6), 175.
[18] Dushimimana A, Niyonsenga AA, Nzamurambaho F (2021). A review on strength development of high performance concrete. Construction and Building Materials, 307, 124865.
[19] EFNARC (2005). The European Guidelines for Self-Compacting Concrete Specification, Production and Use [Internet]. 2005. Available from: https://www.theconcreteinitiative.eu/images/ECP_Documents/EuropeanGuidelinesSelfCompactingConcrete.pdf
[20] Elsebaei M, Mavroulidou M, Micheal A, Centeno MA, Shamass R, Rispoli O (2025). Dealuminated Metakaolin in supplementary cementitious material and Alkali-Activated systems: A review. Applied Sciences, 15(15), 8599.
[21] Harikaran M, Gokulakannan S, Loganathan A, Chandiran R, Ajith M, Dhanasekar V (2023). Metakaolin cement concrete evaluation using industrial by-products as fine aggregate. Materials Today: Proceedings.
[22] Jing H, Li M, Zhang Y, Gao M (2023). Hydration kinetics, microstructure and physicochemical performance of metakaolin-blended cementitious composites. Construction and Building Materials, 408, 133756.
[23] Khatib JM, Clay RM (2004). Absorption characteristics of metakaolin concrete. Cement and concrete Research, 34(1), 19–29.
[24] Morales Fournier J, Acosta Álvarez D, Alonso Aenlle A, Tenza-Abril AJ, Ivorra S (2020). Combining reclaimed asphalt pavement (RAP) and recycled concrete aggregate (RCA) from Cuba to obtain a coarse aggregate fraction. Sustainability, 12(13), 5356.
[25] Mubaraki M, Osman S, Sallam H (2019). Effect of RAP content on flexural behavior and fracture toughness of flexible pavement. Latin American Journal of Solids and Structures, 16.
[26] Rao PM, Raja KH (2017). Study of the properties of metakiolin and GGBS based geopolymer concrete. International Journal of Civil Engineering & Technology, 8.
[27] Shah HA, Yuan Q, Akmal U, Shah SA, Salmi A, Awad YA, et al (2022). Application of machine learning techniques for predicting compressive, splitting tensile, and flexural strengths of concrete with metakaolin. Materials, 15(15), 5435.
[28] Siddique R, Klaus J (2009). Influence of metakaolin on the properties of mortar and concrete: A review. Applied Clay Science, 43(3-4), 392–400.
[29] Sun J, Dong H, Wu J, Jiang J, Li W, Shen X, et al (2021). Properties evolution of cement-metakaolin system with CSH/PCE nanocomposites. Construction and Building Materials, 282, 122707.
[30] Tiza MT, Imoni S, Akande EO, Mogbo O, Jiya VH, Onuzulike C (2024). Revolutionizing infrastructure development: Exploring cutting-edge advances in civil engineering materials. Recent Progress in Materials, 6(3), 1–68.
[31] Zaribaf BH, Uzal B, Kurtis K (2015). Compatibility of superplasticizers with limestone-metakaolin blended cementitious system. Calcined Clays for Sustainable Concrete: Proceedings of the 1st International Conference on Calcined Clays for Sustainable Concrete,.
[32] Zunino F, Scrivener K (2024). Reactivity of kaolinitic clays calcined in the 650° C–1050° C temperature range: towards a robust assessment of overcalcination. Cement and Concrete Composites, 146, 105380.
How to cite this paper
@article{1725546,
author = {Ahmad Alkali Kakashehu, Mohammed Abdulmumin Nda, Abdulmumin Ahmed Shuaibu},
title = {Investigating the Effect of Metakaolin on the Flow, Compressive Strength and Water Absorption of High Performance Concrete},
journal = {Iconic Research And Engineering Journals},
year = {2026},
volume = {10},
number = {5},
pages = {5164-5175},
issn = {2456-8880},
url = {https://www.irejournals.com/formatedpaper/1725546.pdf},
abstract = {High performance concrete (HPC) requires high binder contents, thereby increasing cost and CO₂ emissions. Metakaolin (MK) from locally available kaolin is a promising partial cement replacement, but its interaction with superplasticiser, water-cement ratio and aggregate-cement proportions in Portland-limestone cement HPC has not been fully investigated. This study examined the combined effect of five mix variables on the fresh, mechanical and durability properties of MK-HPC and identified mixes balancing flow, strength and impermeability. A five-factor, five-level central composite design (60 runs) varied MK (5-15% cement replacement), PCE superplasticiser (1.00-1.20%), water-cement ratio (0.31-0.35), coarse to fine aggregate ratio (0.60-1.00) and cement to fine aggregate ratio (1.10-1.50), using cement and metakaolin. Slump flow, 28-day compressive strength and water absorption of HPC were determined. The results revealed that slump flow ranged from 665 to 730 mm, placing every mix within EFNARC class SF2. Compressive strength ranged from 20.9 to 55.3 MPa, while water absorption value ranges from 0.09-1.17%. Concrete specimen that had 28 days compressive strength above 55 N/mm² was achieved by mixes containing (MK= 10-12.5%, SP = 1.1-1.15%, W/C = 0.32-0.33, CA = 0.9-1.0, CE = 1.3-1.4).},
keywords = {central composite design, compressive strength, high-performance concrete, metakaolin, polycarboxylate superplasticizer},
month = {November},
}